In my class in college, the instructor said that the application of the glaze should not be so thick that it pin holes or cracks. Today I applied glaze on a lot of pots and some of the glazes seemed too thick, but being a bit thick myself, I did not add water to them. There were pin holes and cracks in the glaze applications.

 

When they were dry I rubbed with my fingernail to fill in the cracks and pin holes. I guess I could wait the week and a half to answer this question myself, but being an impatient potter, I am so anxious to know it I have messed it all up or if everything is just fine.

 

The glazes were cone 10, matte yellow, tenmoku, ohata, oribe, moonlight, oatmeal and a few others.

 

What do you think? Thanks.

Share this post


Link to post
Share on other sites

In my class in college, the instructor said that the application of the glaze should not be so thick that it pin holes or cracks. Today I applied glaze on a lot of pots and some of the glazes seemed too thick, but being a bit thick myself, I did not add water to them. There were pin holes and cracks in the glaze applications.

 

When they were dry I rubbed with my fingernail to fill in the cracks and pin holes. I guess I could wait the week and a half to answer this question myself, but being an impatient potter, I am so anxious to know it I have messed it all up or if everything is just fine.

 

The glazes were cone 10, matte yellow, tenmoku, ohata, oribe, moonlight, oatmeal and a few others.

 

What do you think? Thanks.

 

 

I think if its really thick a few of those glazes will look like dry cracked lake beds-some of the matts may like a bit thicker application

Those high iron glazes will be darker and can run real thick-oribe is one that needs to be just right with thickness.

One thing is you will learn from this straight away. Nothing like mistakes to learn faster. If you want you can wash all the glaze off with water-let pot dry one day and reglaze with same thinner glaze.Thats what I do when i drop a pot into bucket as a mistake.

I assume this is all on stone ware clay??

Mark

Share this post


Link to post
Share on other sites

In my class in college, the instructor said that the application of the glaze should not be so thick that it pin holes or cracks. Today I applied glaze on a lot of pots and some of the glazes seemed too thick, but being a bit thick myself, I did not add water to them. There were pin holes and cracks in the glaze applications.

 

When they were dry I rubbed with my fingernail to fill in the cracks and pin holes. I guess I could wait the week and a half to answer this question myself, but being an impatient potter, I am so anxious to know it I have messed it all up or if everything is just fine.

 

The glazes were cone 10, matte yellow, tenmoku, ohata, oribe, moonlight, oatmeal and a few others.

 

What do you think? Thanks.

 

 

Did you wash the pottery before hand with a damp sponge? This usually will cut the absorption rate of the glaze and even out the application with a thinner coat than a dry pot. As Mark said you may wash the pot completely and re-glaze. I realize that these pieces are your "babies" so if you have the time-re glaze.

Share this post


Link to post
Share on other sites

The issue is not the cracks or pinholes- rubbing them out won't matter. They are simply indicators that the glaze has been applied too thickly. The real issue is that the glazes will likely run, and possibly end up on the kiln shelf. The thicker the glaze, the more it runs (generally). Wash them off, let them dry completely, and try it again.

Share this post


Link to post
Share on other sites

Thank you for your helpful answers. Yes they are all stoneware and I did sponge them off first. When I get back to school on Monday they won't have been fired yet so I am going to heed your advise and wash them all off. Especially since on the lips I had the inside glaze layered over the outside glaze and then I had little dips of a third glaze and I also used a slip trailer bulb to decorate lightly with another glaze towards the top.

 

Fortunately the crit is on Wednesday and they wouldn't be out of the kiln by then anyway. We are able to use greenware or bisque in the crits since there is such a huge number of pots that are assigned. I think the instructor wants to make sure that students don't view this as a goof-off class, so he really puts the pressure on. But I notice he grades very kindly if you're doing lots of work.

 

I now need to use this experience to learn how thick the glaze in the bucket should be. Using the finger dip method. Thanks.

Share this post


Link to post
Share on other sites

I make my students wash off the thickly applied glazes so they won't run onto the shelves. They are suppose to check the glaze consistency before glazing. Add water if needed. My test is to stir the glaze, then stick a dry finger in the glaze and check the knuckle. One should see lines of the knuckle. It is an old-fashion method but it works.

I have demonstrated this in class.

My recommendation is to wash off the thick glaze. Let the pot dry a day or so and then reglaze it.

 

Marcia

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.