Posted 18 April 2012 - 10:22 PM

I have tissue and wish to print an image or text onto it. Then transfer this onto the clay.

The ones I currently use are pre printed, These are placed onto the clay the back is brushed with water then tissue is peeled away>

Thanks



Mike

#2 INYA

INYA

    Advanced Member

  • Members
  • PipPipPip
  • 87 posts
  • LocationSlovenia, Europe

Posted 20 April 2012 - 12:12 PM

and your question is?
.......................

skratblog.blogspot.com
www.skrat.eu

#3 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,326 posts
  • LocationRed Lodge, Montana

Posted 21 April 2012 - 07:18 AM

I agree with INYA.
What is your question?
Marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#4 Raku

Raku

    Member

  • Members
  • PipPip
  • 16 posts
  • LocationPerth Western Australia

Posted 27 April 2012 - 07:58 PM

and your question is?




Have tissue and wish to print an image or text onto it. Then transfer this onto the clay ?

Ok, how do I preint the image onto the tissue, Prefer Printer if possible. Any ideas on the type of Ink???



Regards

#5 Raku

Raku

    Member

  • Members
  • PipPip
  • 16 posts
  • LocationPerth Western Australia

Posted 27 April 2012 - 07:58 PM

I agree with INYA.
What is your question?
Marcia



Have tissue and wish to print an image or text onto it. Then transfer this onto the clay ?

Ok, how do I preint the image onto the tissue, Prefer Printer if possible. Any ideas on the type of Ink???



Regards

#6 Mark C.

Mark C.

    Advanced Member

  • Members
  • PipPipPip
  • 6,303 posts
  • LocationNear Arcata Ca-redwood rain forest

Posted 27 April 2012 - 08:48 PM

This has been covered-use the search or google it-I recall printer details etc.
Mark
Mark Cortright
www.liscomhillpottery.com

#7 Raku

Raku

    Member

  • Members
  • PipPip
  • 16 posts
  • LocationPerth Western Australia

Posted 28 April 2012 - 06:59 PM

This has been covered-use the search or google it-I recall printer details etc.
Mark



ive searched and found nothing
Google only comes up with pre printed or the sliding type transfer.



Thanks

#8 icyone

icyone

    Advanced Member

  • Members
  • PipPipPip
  • 65 posts

Posted 28 April 2012 - 09:59 PM


This has been covered-use the search or google it-I recall printer details etc.
Mark



ive searched and found nothing
Google only comes up with pre printed or the sliding type transfer.



Thanks

think they meant search here on forum too

#9 bciskepottery

bciskepottery

    Advanced Member

  • Moderators
  • 2,703 posts
  • LocationNorthern Virginia

Posted 28 April 2012 - 10:09 PM

Mitch Lyons applies colored slip to newsprint, then transfer it to clay slabs. He has a video demonstrating the process.

Here is another approach:

#10 Raku

Raku

    Member

  • Members
  • PipPip
  • 16 posts
  • LocationPerth Western Australia

Posted 29 April 2012 - 01:38 AM

Mitch Lyons applies colored slip to newsprint, then transfer it to clay slabs. He has a video demonstrating the process.

Here is another approach: http://www.youtube.c...h?v=mDzaBwxeuhg



Thsi is NOT Slip.