What rutile to get?

Recommended Posts

I'm going to be experimenting with a new glaze from John Hesselberth book and it calls for rutile. I get my supplies from the Clay Art Center in Seattle and they have two diifferent ones, one is milled ( thinking this is the one) and the other it says is "ceramic rutile", say's it should be screened before using due to various sized particles. I'm assuming that I need the milled rutile, but wanted to make sure.

 

 

Thanks for the help.

 

Bob

Share this post


Link to post
Share on other sites

You want the fine rutile-probably milled. You can also buy granular Rutile which is used to put "iron" spots in glazes when you fire in an electric kiln.It is a coaser grind and would have to be seived out if you want a smooth glaze

TJR

Share this post


Link to post
Share on other sites

I looked up my records-I get my rutile by the 50# bag from Laguna Clay Co.

 

They sell 3 types

 

Milled

 

Ceramic Grade-which is plenty fine

 

Granular –which looks sort of darkish

 

I have been using ceramic grade for 30 years as I go thru lots

 

The brands have changed over the years but its all been ceramic grade for me.

 

I just check both my bags and they are really fine powder.

 

Your supplier may have only two kinds

 

Mark

Share this post


Link to post
Share on other sites

Thanks for the responses. I'm looking at making a smooth glaze so the milled would work the best. But, I've also been interested in adding to a glaze to add iron spots to it. I think I will buy the ceramic grade and screen it to take out the larger pieces to use later.

 

Thanks again.

 

Bobg

Share this post


Link to post
Share on other sites

Thanks for the responses. I'm looking at making a smooth glaze so the milled would work the best. But, I've also been interested in adding to a glaze to add iron spots to it. I think I will buy the ceramic grade and screen it to take out the larger pieces to use later.

 

Thanks again.

 

Bobg

 

 

Bobg;

I don't know if you are familiar with Dansk Pottery. They make a high end stoneware dinner plate in Albany slip colour[brown] and a white matt that has speckles. They are fired in oxidation in an electric kiln. [i think]. Potters add speckles to their glazes to get that stoneware reduction effect. You can use granular rutile, and you can also use granular illmanite. Don't quote me, but I think 2% would give you the effect you are looking for.I do not use these techniques in my own work, but remember them from art school.Good luck.

TJR.

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.