I have a vanadium underglaze recipe that changes color from yellow to green (only wet in the container, it  fires yellow).  The color shift makes mixing colors difficult, and I’m hoping someone here has a solution to curb the growth of whatever microbes are changing its color. 

Share this post


Link to post
Share on other sites

bleach works.  just a little unless the staining has spread throughout the liquid.   happens with my slips which i use for several years and i just bleach it out.

Share this post


Link to post
Share on other sites

Is firing the bleach hard on the kiln elements?  Chlorine gas is pretty corrosive, no?  Is the amount used not enough to cause problems?

 

Share this post


Link to post
Share on other sites

I make it and it lives in a windowless room, in an opaque container, so I guess you’re right and it’s probably some other microorganism, not algae.  Whatever it is, it only lives in the vanadium underglaze, none of the other mason stains seem to change color, but the base does bubble when it’s freshly made like it’s fermenting!   I’m going to try some vinegar and see if a ph change is enough to make it less appealing to the buggers. 

Share this post


Link to post
Share on other sites

@Lbegley, a tiny bit of copper carbonate added to brushing medium stops the gums in the brushing medium from rotting, magma glaze additive suggests using copper also. The amount used is so small that it doesn't effect the colour. Same principle would apply to underglazes as glazes. By weight it would be 0.04% copper carbonate, like everything ceramics, if you try this test a small amount first.

Share this post


Link to post
Share on other sites

 

5 hours ago, Min said:

@Lbegley, a tiny bit of copper carbonate added to brushing medium stops the gums in the brushing medium from rotting, magma glaze additive suggests using copper also. The amount used is so small that it doesn't effect the colour. Same principle would apply to underglazes as glazes. By weight it would be 0.04% copper carbonate, like everything ceramics, if you try this test a small amount first.

Thank you!  I will test copper carb. 

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.


×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.