10 hours ago, Babs said:

Is there a ferro fri equivalent of the above frit?

Not that I know of. Try posting the recipe and maybe someone can re-do it with what frits you have on hand.

Share this post


Link to post
Share on other sites

Thanks Min

It's a Black Satin glazy.org glaze.

I didn't record Name as I was taking screen shots..

Anyway

Soda Feld.                   26

Crecer frit 804.       26

Silica.                              23

Dolomite.                    14

Kaolin                            11

+

Bentonite.  2

Copper Ox.  2

RIO.                  1

 

 

Share this post


Link to post
Share on other sites

If anyone has a minute would you mind checking my calc as I've had a few funny things happening lately with Insight. I think it's okay but would appreciate someone double checking the figures.

It's not perfect but I was trying to keep the ingredients to basic ones, so I didn't use Fusion frit F43. No guarantees (test before using it on real pots please, also check for leaching ). I just used theoretical numbers for soda spar as I don't know which one you use Babs.

 1418983312_ScreenShot2019-03-05at7_26_56PM.png.354abb6817395239861456d472b4ed2c.png

Share this post


Link to post
Share on other sites

@Min thank you. I will test over next week.

My Soda Feld .unknown to me I inherited a garbage bin full along with bins full of other basic materials.

I have Ferro frit 3134 which is sold as ff4108 for no apparent reason...

I'll post results.

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.