Sissy owens Posted February 24, 2019 Report Share Posted February 24, 2019 I just bought an Olympic electric kiln series 700. I bisque fires and my pots came out great. Then i glazed my pots and put in kiln and selected slow glaze at cone 6 opened it this morning and they changed to a dark color and that’s it what happens? Link to comment Share on other sites More sharing options...
Min Posted February 24, 2019 Report Share Posted February 24, 2019 Hi Sissy and welcome to the forum. It would help if you could post a picture of the pots and give more information about the clay and glaze(s) used. Link to comment Share on other sites More sharing options...