Black Luster is my student's favorite glaze to use. I bought more of it but it arrived very chunky and not like normal glaze chunky-the chunks are hard. I put it through a blender and it broke up the chunks a little but then they reformed. I read that sometimes glazes can get chunky when it is too cold but none of the other glazes we have are doing it. ??