On impulse ,  I bought a bag of nickel sparkles. There is no information about what cone range they would work at. I've written the manufacturer and have not gotten an answer.  I sprinkled them on a couple different glazes and fired them  at ^6 oxidation. That was obviously way too hot. On one glaze they did absolutely nothing . On the other glaze they spatter the glaze all over and made an ugly mess.

,

Does anyone know how hot you can fire these things?

Share this post


Link to post
Share on other sites

I was referring to liambesaw  writing it spat glaze everywhere.

I had a pink blue nickel containing glaze which did just that and when a bit landed on an element...curtains for that element.

Glaze my used after that but was an Interesting glaze

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.


×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.