Is it possible to make a plaster hump mold of a straight sided, deep Tuperware type container? I've tried it once, using Murphy's oil soap as a release agent but I can't get the plaster hump out without cutting off the plastic bowl. Any tips?

Ann B

Share this post


Link to post
Share on other sites

I use something called 'soft soap', not really a soap, but must be similar to what you already use. I've heard of some using the can spray cooking oil but I have never tried it. Good luck

Share this post


Link to post
Share on other sites

Is it possible to make a plaster hump mold of a straight sided, deep Tuperware type container? I've tried it once, using Murphy's oil soap as a release agent but I can't get the plaster hump out without cutting off the plastic bowl. Any tips?

Ann B

 

No art without sacrifice. The tupperware will go to its reward knowing it gave its life in a good cause.

Petroleum jelly might do the trick.

Share this post


Link to post
Share on other sites

Strait sides = friction and drag.

You can try "Burping" the mold. This is where you use compressed air to pop the seal between mold and master.

Other wise, cut the bowl.

Share this post


Link to post
Share on other sites

If there are no undercuts, petroleum jelly should work... at least it seemed to work well for making bronze casting molds from plaster. Normally one uses something with a slight inward slant to make releasing a bit easier.

Share this post


Link to post
Share on other sites

Is it possible to make a plaster hump mold of a straight sided, deep Tuperware type container? I've tried it once, using Murphy's oil soap as a release agent but I can't get the plaster hump out without cutting off the plastic bowl. Any tips?

Ann B

 

 

I use baby oil. It hasn't failed me yet.

Brenda

Share this post


Link to post
Share on other sites

Just a thought, but I like to use bisque molds. That is, if you're hand building--if you're pouring, then never mind . . . . I just throw a piece the size and shape I want, then trim the outside to be nice and smooth. That way I can coil/puzzle/pound my clay over the outside or make a smaller piece on the inside.

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×