We are looking for cone 10 stoneware reduction body with good thermal shock properties.

#2 pyroteacher

pyroteacher

    Member

  • Members
  • PipPip
  • 10 posts
  • LocationRogers, Arkansas

Posted 24 May 2010 - 03:30 PM

B-Mix!
Old potters never die, they just slip away....

#3 GEP

GEP

    Moderator / full time potter ^6 stoneware

  • Moderators
  • 1,354 posts
  • LocationSilver Spring, MD

Posted 24 May 2010 - 03:45 PM

Laguna 901 is a very dark, high-iron clay. The iron can make the clay unpredictably brittle, especially when overfired. So choose something that is lighter in color. This doesn't mean your pots will turn out light, they might still flash dark in reduction.

My favorite cone 10 stoneware for reduction ... Highwater's Phoenix.

-Mea
Mea Rhee
Good Elephant Pottery
http://www.goodelephant.com

#4 AndyL

AndyL

    Advanced Member

  • Members
  • PipPipPip
  • 165 posts
  • LocationNJ, USA

Posted 24 May 2010 - 05:16 PM

I've used Standard Ceramic Supply #306 Stoneware http://standardceram...hFireClays.html and find it pretty forgiving. At the College I've taken courses in they even use it for Raku.