WD40 is a very thin lubricant, but most of it just evaporates out, "WD" stands for "water displacement" and it was invented after 40 trials and errors to get a formula that would displace moisture and water and lubricate with the properties the manufacturer wanted.

 

Oil is oil basically, it's all petroleum, but too thin will evaporate out, too thick might not get in where it needs to go. I would try some "3 in 1" oil, or light machine oil and let it sit, if you can get ANY movement at all in either direction then work it back and forth repeatedly quickly, and add more of the oil in all the holes as it gets looser and looser.

 

What's probably happened is the bearings' lubricant has dried out and then the steel balls, sleaves or some other parts in there have rusted, and rust expands.

If there's any holes large enough, it's also possible some insects have managed to get in and nest a bit, which can bring in moisture, grit, dirt etc too.

 

I had this happen to a bearing in a dust collector motor, and I opened the motor up and was able to get some oil in the rusted bearing in the back of it, and working it back and forth it loosened up, adding more oil helped flush the crud and disolved rust out and after flushing it with more oil and wiping, it worked fine and I still use it with no trouble.

 

Share this post


Link to post
Share on other sites

Dear MichaelS,

 

I had thought I had no hope of getting to Ikea, but my daughter says there is one near her and I am off to see my grandchildren for their half-term holiday tomorrow, so she will take me to Ikea! They do have the lazy susans in stock, according to their website, so that should solve the problem - thanks a lot! (I'll still try to loosen the banding wheel, eventually)

Idaho Potter likes this

Share this post


Link to post
Share on other sites

Is it possible that something was put inside to stop it from spinning, temporarily? Did you check the bottom? Is there a screw on the side that could possibly have been tightened to stop the spinning?

I agree with Marcia I can't imagine a banding wheel doing this. Do a search of the manufacturer so you can inquire of them. There couldn't be many who make bright blue banding wheels!

 

Share this post


Link to post
Share on other sites

Dear Lucille Oka,

Thank you for your reply. I'm afraid it is a cheaper model with no screws or manufacturer's name. Just stuck. I will try putting the oil on and leaving it upside down as some people have suggested. Meanwhile I hope to do as MichaelS suggested and buy a lazy susan at Ikea.

 

I liked the message in Latin! (my Latin was never very good, but I did manage to translate it! It helped that I knew that wonderful message in English!)

Share this post


Link to post
Share on other sites

Well, considering the apparent fall out over the WD40 comments I think I should post why I said what I said. I checked to see what the official WD40 site had to say about it's product and the site does say that WD stands for Water Displacement and that it is a lubricant. That is their official statement. Anyway going back in time many years I was the Chief Operating Officer of Action Hydraulics, Inc., located at 800 51st Ave in Oakland, CA. We held several classificatino numbers and some of our information is still on the web. Action Hydraulics was a military aerospace contractor and we used to manufacture parts for installation on the Atlas-Centaur Launch Vehicle. the pictures of the launches where one could see the hoses cables that drop off the launch vehicle, well those hoses and cable swere one of our products. We also manufactured a number of other items including the hydraulics for the APECS ship-board protection system. one of the products we had to use on all our equippment was a product that was supplied to us by the Boeing Corporation and it was designated WD40 and was a washdown prior to packaging and shipping various components. In discussions with Boeing engineers it was said that the washdown was the same as the WD40 sold over the counter.

 

Reading the website of WD40 they make a lot of statements but they give little in the way of hard facts. They claim that WD40 is a penetrant and a lubricant but they have no lubricity data and certainly no data to indicate it use a s penetrant. They state their formula is secret.

 

I still believe the advice I gave regarding the use of kerosene or diesel as being a better penetrant is sound and I would not recommend something as volatile as WD40 as a lubricant for rotating machinery and that is based on sound and experienced engineering. I have no idea what happened subsequent to my post.

 

Best regards,

Charles

Share this post


Link to post
Share on other sites
Guest ---

Well, considering the apparent fall out over the WD40 comments I think I should post why I said what I said. I checked to see what the official WD40 site had to say about it's product and the site does say that WD stands for Water Displacement and that it is a lubricant.

 

I still believe the advice I gave regarding the use of kerosene or diesel as being a better penetrant is sound and I would not recommend something as volatile as WD40 as a lubricant for rotating machinery and that is based on sound and experienced engineering. I have no idea what happened subsequent to my post.

 

Best regards,

Charles

 

 

Charles, your post was not the problem, I had simply replied to it and this portion in particular;

 

"WD40 is an aerospace wash-down formula whence the WD in the WD40."

 

I had said "WD" stood for Water Displacement, and that it was their 40th formula try- all taken from their website which I read years ago. I had simply said oil is oil, it's all petroleum, and that one can use a light machine oil or "3-in-one" oil and soak the bearings which appeared from the description to have seized up from rust.

That's about all I said, and I came back a little while later and find my post "rating" voted DOWN into the negative numbers anonymously so I thought what the hell? and then I thought well the heck with this I don't need to spend my time finding, writing out information, posting, and having people hit the negative rating buttons as some kind of "protest slam" joke, or whatever.

 

That's the problem with those ratings features or "karma" on another one- on some of these board software packages, posting on an art site shouldn't become a built-in competition to gain the most "like" points, highest score, highest post count, "most karma" or most pats on the back, unfortunately the software here has this function built-in and I haven't seen this function in years, SMF and vBulletin do not have it.

 

In any case I'm going back to maintaining the other art site as the owners fixed the robo-spam problem and intend to keep it up instead of abandoning as they appeared to be going towards.

 

Take care.

AmeriSwede likes this

Share this post


Link to post
Share on other sites

Well, considering the apparent fall out over the WD40 comments I think I should post why I said what I said. I checked to see what the official WD40 site had to say about it's product and the site does say that WD stands for Water Displacement and that it is a lubricant.

 

I still believe the advice I gave regarding the use of kerosene or diesel as being a better penetrant is sound and I would not recommend something as volatile as WD40 as a lubricant for rotating machinery and that is based on sound and experienced engineering. I have no idea what happened subsequent to my post.

 

Best regards,

Charles

 

 

Charles, your post was not the problem, I had simply replied to it and this portion in particular;

 

"WD40 is an aerospace wash-down formula whence the WD in the WD40."

 

I had said "WD" stood for Water Displacement, and that it was their 40th formula try- all taken from their website which I read years ago. I had simply said oil is oil, it's all petroleum, and that one can use a light machine oil or "3-in-one" oil and soak the bearings which appeared from the description to have seized up from rust.

That's about all I said, and I came back a little while later and find my post "rating" voted DOWN into the negative numbers anonymously so I thought what the hell? and then I thought well the heck with this I don't need to spend my time finding, writing out information, posting, and having people hit the negative rating buttons as some kind of "protest slam" joke, or whatever.

 

That's the problem with those ratings features or "karma" on another one- on some of these board software packages, posting on an art site shouldn't become a built-in competition to gain the most "like" points, highest score, highest post count, "most karma" or most pats on the back, unfortunately the software here has this function built-in and I haven't seen this function in years, SMF and vBulletin do not have it.

 

In any case I'm going back to maintaining the other art site as the owners fixed the robo-spam problem and intend to keep it up instead of abandoning as they appeared to be going towards.

 

Take care.

 

 

I certainly hope you do not decide to leave this discussion group because it has been my experience that many of the posters here are not only professionals but some of the best educators in the business. People like John Baymore, Marcia Selsor, Chris Campbell and Stephen Robison are an incredible resource to find anywhere let alone in one area. Many of the other posters are professionals who have been actually creating in ceramics for many years and also have a wealth of information to share and they all share it selflessly.

 

Unfortunately in an community there are a certain number of people who are petty, picayune and just generally un-nice people. Many years ago I had a co-worker who had a motto: "Illigitimi non carborundum" don't let the bastards wear you down. Now I know that there are some who will jump on this as lousy Latin and there are those who can only pick on one's spelling (or typing. or grammar) and this applies to them too! But don't give up a valuable resource. Like any other community one has to spend a little time to determine whose posts are treasure and whose posts a garbage. I believe that you will find more value here than angst.

 

I hope to see you around.

 

Best regards,

Charles

 

 

 

Share this post


Link to post
Share on other sites

Dear MichaelS,

 

I had thought I had no hope of getting to Ikea, but my daughter says there is one near her and I am off to see my grandchildren for their half-term holiday tomorrow, so she will take me to Ikea! They do have the lazy susans in stock, according to their website, so that should solve the problem - thanks a lot! (I'll still try to loosen the banding wheel, eventually)

 

 

 

Something that is obvious (once you have done it) they work just as well upside down and are very stable that way....they are also very sturdy......I currently have 15 kg of coiled clay sitting on one and it is smooth operating and steady.

I actualy use them more than my "real" banding wheel now.

Good luck and let me know how they work out for you.

 

Ps ,, where are you based,,,I am in Derbyshire.

 

Michael

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×