Hi,

I have a couple of glazes made up and I want  to be able to brush on as I'm having difficulty dipping. How so I do this?

Many thanks

Best regards 

Andrea

Share this post


Link to post
Share on other sites

Hi Andrea, 

Is brushing medium available where you live? First off you need to remove some of the water from your dipping glaze, by evaporation and/or decanting some off the top (if soluble materials in glaze you will loose a little this way), try and get about 1/3 of the water out of the dipping glaze. Then either add some commercial brushing medium as per directions or mix up some of your own. For making your own take a gallon of very hot water and sprinkle on 2 tablespoons of CMC gum plus an optional 1 tablespoon Veegum T (or if you have it just use Veegum Cer in place of both those)  plus a 1/4 teaspoon of copper carb. (copper will stop the gum from rotting). Let it sit overnight then mix it up with a stick blender. Add a bit of the gum solution to your glaze, try brushing it, add more if necessary. 

edit: what is the difficulty with your dipping glaze?

Edited by Min
added a question

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now

×

Important Information

By using this site, you agree to our Terms of Use.