Hahahahha, I know I know, lol. 

 I bought someone's entire small studio this morning and nothing has been used in like 3 years, it all stinks of mildew and I have it completely torn down laying in the driveway soaking up some sun. Can I leave it and the shelves/stands/peephole covers/temp cones, etc.. overnight with heavy dew and dry all day tomorrow? It will not be plugged in for 2 or 3 weeks, I just want to air it all out before bringing it inside.

Share this post


Link to post
Share on other sites

NO!!!!!!!!!!                                                                                                                                                                                                                                                                                                                                                                                       

Share this post


Link to post
Share on other sites

Tarp it for the night-keep the dew off -untarp in am and let dry-do not let it get wet again.The idea is to dry it out from this point forward.Tarps are cheap-even cardboard will work for. night or two.

Edited by Mark C.

Share this post


Link to post
Share on other sites

Shawnhar - For your first firing, you might want to run a slow firing to gently drive off any accumulated moisture, much like you would do upon receipt of a brand new kiln. 

Here's a link to the L and L Jupiter Kiln manual which has information on firing up a kiln for the first time .  About 15 pages into the document you'll find the manual firing instructions for that first fire.  Instructions using an automated controller (Dynatrol) are another 12 or so pages below that.). 

https://hotkilns.com/sites/default/files/pdf/BookJupiterManual 9-26-11.pdf

-S. Dean

Share this post


Link to post
Share on other sites

When cones get wet they can be affected-as Min said. You should test them against dry good cones.The rest of the stuff can dry out without harm. The electric panel on kiln needs to be very dry before energizing.

 

Share this post


Link to post
Share on other sites

Thanks all!

I don't think it was clear from my post but I meant wet from dew, everything is bone dry and nothing has been wet.

I brought the kiln inside last night and the smell is mostly gone. The wheel is the worst smelling and I left it out last night, made sure everything else was under a patio umbrella to keep the dew off.

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.