Hi all,

i know how to make three footed, “tripod” pottery such as the kind Sandi Pierantozzi makes, as I bought her video here. I may have asked this already, but how do you make feet like that with 4 feet? 

These are tripods on etsy: 

https://www.etsy.com/market/tripod_mug

I've been playing with it, and I don’t think you can do the same technique. I was thinking of maybe cutting away clay fromthe bottom? Any ideas, much appreciated!

Nancy

Share this post


Link to post
Share on other sites

Hi Nancy,

Are you trying to do the pinching method or the foot-ring method? With the pinching method, instead of a triangle, you would have to squeeze a square and then pinch the corners. I would pinch opposite corners first and then do the same with the remaining corners until you bring the bottom together. I think the footring method is easier. You just have to be accurate with your layout of the 4 feet. you would form your pot with a bottom thick enough to trim a footring to the height that you desire or do a flat-bottomed pot and add a footring of the desired height, layout the 4 feet and carve away what you don't want. I've used the first footring method for making my berry bowls. 

The primary reason for doing three footed pots is for stability. Tripods are a lot more stable than quadpods.

Hope this helps...

JohnnyK

Share this post


Link to post
Share on other sites
1 hour ago, JohnnyK said:

Hi Nancy,

Are you trying to do the pinching method or the foot-ring method? With the pinching method, instead of a triangle, you would have to squeeze a square and then pinch the corners. I would pinch opposite corners first and then do the same with the remaining corners until you bring the bottom together. I think the footring method is easier. You just have to be accurate with your layout of the 4 feet. you would form your pot with a bottom thick enough to trim a footring to the height that you desire or do a flat-bottomed pot and add a footring of the desired height, layout the 4 feet and carve away what you don't want. I've used the first footring method for making my berry bowls. 

The primary reason for doing three footed pots is for stability. Tripods are a lot more stable than quadpods.

Hope this helps...

JohnnyK

Hi JohnnyK,

Yes, that is what I'm trying to do - the pinching method. But I have seen the footring method too, but couldn't look it up, cause I didn't know what it was called! So you make a thick bottom, then carve the upward curve into it? I will go check to see if I can find some videos to help me see it, also. Thank you very much,

Nancy

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now

×

Important Information

By using this site, you agree to our Terms of Use.