If the surface is smooth, you should be able to do the glaze over. How are you applying? Brushing will require some work, but is probably the same as bisque or pretty close, Spraying will work well as long as you don't saturate, and dipping may take heating up the pot in the oven a bit before dipping.

 

best,

Pres