Wondering if anyone has a celedon type of glaze for ^6 in an electric kiln.

#2 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,144 posts
  • LocationRed Lodge, Montana

Posted 13 July 2010 - 07:59 AM

Wondering if anyone has a celedon type of glaze for ^6 in an electric kiln.

My celedon is a combination of two glazes. You need to adjust the combo to the color you like. Since I have these mixed up already I ended up combining 3 parts Faux celedon to 2 parts Mizuno. The Faux celedon is a fat glaze. The Mizuno is a shiney clear. I was doing color tests to match a ^10 reduction celedon.
Faux Celedon

Whiting 18.5

Neph Syen 25.8

EPKaolin 18

Silica 31.5

Gerstley Bor 4.6

97.4



add to Faux base

0.5 copper Carbonate

0.025 Black Stain 6600

0.02 iron oxide




Mizuno Clear



Whiting 7

Zinc OX. 5

Kaolin 9

Silica 21

Gerstley B 8

Talc 2

F-4 spar 48

100




The final result was identical to a celedon I tweaked in Hawaii ^10 REDUCTION.
Hope this is of some use. I will eventually work out the combined recipe when I go to mix glazes next time. But here it is as I am now using it.
Marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#3 hansen

hansen

    Advanced Member

  • Members
  • PipPipPip
  • 121 posts
  • LocationAlexandria, Virginia

Posted 15 July 2010 - 06:08 AM

everytime something like this is posted I have to archive it.

But THANKS!!! anyway

: )

h a n s e n


Wondering if anyone has a celedon type of glaze for ^6 in an electric kiln.

My celedon is a combination of two glazes. You need to adjust the combo to the color you like. Since I have these mixed up already I ended up combining 3 parts Faux celedon to 2 parts Mizuno. The Faux celedon is a fat glaze. The Mizuno is a shiney clear. I was doing color tests to match a ^10 reduction celedon.
Faux Celedon

Whiting 18.5

Neph Syen 25.8

EPKaolin 18

Silica 31.5

Gerstley Bor 4.6

97.4



add to Faux base

0.5 copper Carbonate

0.025 Black Stain 6600

0.02 iron oxide




Mizuno Clear



Whiting 7

Zinc OX. 5

Kaolin 9

Silica 21

Gerstley B 8

Talc 2

F-4 spar 48

100



The final result was identical to a celedon I tweaked in Hawaii ^10 REDUCTION.
Hope this is of some use. I will eventually work out the combined recipe when I go to mix glazes next time. But here it is as I am now using it.
Marcia




h a n s e n
Stone House Studio, Alexandria, Virginia