Hello.

I may have an opportunity to upgrade my old Bentrup TC66 controller and I'm now choosing between a Stafford ST315B, with 1 ramp + 1 soak per segment,

or the ST316B with 2 ramps + 1 soak per segment.

What are the benefits of having 2 ramps in a segment, assuming I will not be soaking the intermediate temperature before proceeding to the next segment? I mean, I can always input the second ramp as a separate segment, right? Or am I missing something?

 

So if I choose the ST315B, my simple schedule will look like this:

Segment 1: Ramp of 100C/h to 600C (end of segment 1) --don't need to soak

Segment 2: Ramp of 150C/h to 1200C, then hold for xx min/hours --end--

 

If I choose ST316B, it would be like this:

Segment 1: Ramp1 of 100C/h to 600C, Ramp2 of 150C/h to 1200C, then soak (since every end of segment has soak function) --end--

 

Naturally, the higher model will have more functionality but apart from having 1 segment vs 2 when programming the controller, what are the benefits I'm not realising?

 

Thank you.

 

 

 

Share this post


Link to post
Share on other sites

How many segments can you program?

Many potters would have a more gentle 1st segment. 

Then 100C/hr to 600

Then 150 C poss to close to final temp 

Then a slow down to final temp. And a soak.

That would be a glaze firing schedule which would be altered according to contents of kiln....

 

Share this post


Link to post
Share on other sites

Hi Babs.

Both controllers are capable of doing 1-9 segments, their only difference really is the higher end being capable of 2 ramps per segment.

This is where I can't seem to find value in inputting ramp 2 when there's always the option of inputting it as another segment as long as I get to the target temp anyway.

I suppose it would look like an "organised" program, grouping your ramps and all? :mellow:

 

Share this post


Link to post
Share on other sites

To mimic the effect of two ramps per segment just set the hold for segment 1 as 0:00. Like others have said, there's no real benefit of having two ramps in a segment if you have 9 segments available. 

Seg1: 100C/h to 600C; no hold
Seg 2: 150C/h to 1200C; then hold for xx min/hours

is the same as 

Seg1: R1 100C/h to 600C; R2 150C/h to 1200C; then hold for xx min/hours

Edited by Chris Throws Pots

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now

×

Important Information

By using this site, you agree to our Terms of Use.