Hello,

I am fairly new to pottery and lack glazing experience. I am going to have my first experience with dipping (Amaco PC) 

After dipping can I brush small amounts of Amaco PC brushing glaze over the dipped glaze?

thanks to you all for help !! 

S. 

Share this post


Link to post
Share on other sites

Maybe. It depends on the durability of the dipped glaze. If it was a glaze that was mixed for dipping, as in not a watered down brushing glaze, it may not hold up to brushing on top of it- it'll wipe away as you try to brush it. You'll have to test. Brushing glazes have hardeners in them that make them durable enough to brush on top of, so you can do several coats.

Share this post


Link to post
Share on other sites

I see. I am going to dip a tray in Pc Blue midnight and want to put some waves of lighter color on the surface but all I have in a lighter color is jarred brushing glaze.  If I am not too aggressive might it work or could I apply with an applicator?

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.