I've got a bisqued mug with a lot of various underglazes layered over textures on the outside, it's nice. I'm unhappy with the solid underglaze blue on the handle and inside - it wants 'ageing'. Will bisqued underglaze take a watered down underglaze wash OK?   

And for future reference, what about painting undiluted coats of underglaze on bisqued underglaze?

I've only used UGs on greenware. 

I'll be glazing with the usual clear.

Thanks!

Share this post


Link to post
Share on other sites

I think some underglazes are designed to work as well on bisque as on greenware and some not.

The underglazes I use work equally well on greenware and bisque. 

I prefer to underglaze on greenware, because if I underglaze and then glaze in the same stage, on bisque, the clear glaze can smear the underglaze.

Share this post


Link to post
Share on other sites

Thanks! I knew they'd work on bisqued clay,  glad to hear that extends to *underglazed* bisque.   More room to fiddle is always good. 

Quote

 

 

Edited by laughlin

Share this post


Link to post
Share on other sites
17 hours ago, laughlin said:

I've got a bisqued mug with a lot of various underglazes layered over textures on the outside, it's nice. I'm unhappy with the solid underglaze blue on the handle and inside - it wants 'ageing'. 

 

Another approach to aging the handle is to take a walk outside with some sand paper and an x-acto knife and scratch and sand away some of the under glaze.  Use fine sand paper at the end to get rid of any jagged spots. You can still add a wash to this afterwards if it needs it.

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.