Recommended Posts

Hi Everyone,

New to the group and very new to pottery...although my wife has been doing it 35 years.  I was helping her fill an order of 100 plates...the client asked us to stamp

a logo in the middle.  I'm pretty good with a 3D printer....SO...I whipped it up and she's used it on half the order already.  We just realized.  IT'S BACKWARDS.  Very

bad move...but it's subtle.  Can't deliver these to the client.  My question is....since about 25 of these have already been fired and some are still drying....is there any

way to 'fill in' the backwards logo to get rid of it...so at the very least these plates could be sold elsewhere?  Slip, magic....anything?  I feel horrible.  Please let me know

if you have any thoughts.  Thank you.  - Paul

 

PS - THIS IS STONEWARE....not sure if that makes a difference.

Edited by Bits52

Share this post


Link to post
Share on other sites

 

Fish Sauce Slip can be made really quite thick and works on greenware and bisque, I would try that on one that has not been glazed yet to fill it in.

Fish Sauce Recipe ^04 - 10

Kona F4 23.5% (Minspar)

Grolleg 43.6%

Pyrophyllite 7.8%

Bentonite 9.5% ( I use 5 macaloid / bentone MA)

Silica 15.6%

Welcome to the forums :)

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now

×

Important Information

By using this site, you agree to our Terms of Use.