I'm looking for an ultra low-fire clear glaze as I want to dip my toe in kutani yuri-kinsai.. I found an interesting cone 014 recipe that is about 25% frit p-54, and I cant find any for sale online.  Can anyone suggest either a suitable replacement for frit p-54 or an alternate low/fast-fire clear glaze that is suitable for yuri-kinsai?

This is the glaze I was going to roll the dice with:

 

Frit 3269 44    
Frit P-54 26    
Silica 14    
Lithium Carbonate 10    
Kaolin (Theoretical) 6

 

 

thanks all!

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.