I recently received 200 lbs of ferro frit 3110, month back or so. After 20+ attempts! still no crystals. Even the old tried and true recipes produced nothing, not even nucleation sites. I have also noticed it wants to crawl-odd. Crystalline glaze can do very strange things, but crawl or non- nucleation is not among them. Not to mention all four bags were like bags of boulders- rock hard. Anyone else having issues, noticed changes, etc? 

Nerd

Share this post


Link to post
Share on other sites

Are you sure it is 3110, as others have said? If you got it from a crystallier, could it be Fusion 644, which despite its other benefits, has the sad behavior of solidifying in the bag. (I break chunks out with a hammer and chisel, and then grind it in a coffee mill before I can use it.) 

Share this post


Link to post
Share on other sites

Dick:

i have ten pounds of chunky monkey FF 644 out there.

the bags are plainly marked Ferro Frit, but I threw them off the truck without checking ID stamp. Guess I will be looking in the AM.

TY all.

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.