Babs Posted November 23, 2017 Report Share Posted November 23, 2017 mixing late last night, batch now has whiting instead of calcite, gonna glaze tonight, what diff can I expect? Link to comment Share on other sites More sharing options...
Sputty Posted November 23, 2017 Report Share Posted November 23, 2017 . Link to comment Share on other sites More sharing options...
Min Posted November 23, 2017 Report Share Posted November 23, 2017 Tomatoes and tomahtos, but cherry or beefsteak? Difference in particle size effects the melt, example would be wollastonite melting better than calcium carb plus silica. Link to comment Share on other sites More sharing options...
Babs Posted November 23, 2017 Author Report Share Posted November 23, 2017 firing now, will know Sund.a.m. Majolica glaze, pretty forgiving, I slow and soak at end so hopefully...... Link to comment Share on other sites More sharing options...
Babs Posted November 26, 2017 Author Report Share Posted November 26, 2017 All's well with the substitution. Link to comment Share on other sites More sharing options...