3 varieties actually.

1. Yellow zinc from sphalerite ore (Mexico)  80% pure! but also comes in calcined version- Denzox.- up to cone 10.

2. White zinc 99.8% pure zinc oxide: but starts to vaporize above 2260F.

3. Metallic zinc- pure zincite metal. Low fire, can be very reactive if over- fired. Cone 3 or lower pending flux levels.