I slam wedge small amounts of locally dug crushed dry yellow and orange clay into cone 10 porcelain. 

 

Take about a quarter of a 25 pound bag of clay, slice into half inch slabs with a wire tool, sprinkle the dry local clay on the slab, slam another slab on top, sprinkle dry local clay on the top of the stack, slam a pure slab on next, and so on.  Then slam wedge the whole mass about 10 times, then use the clay.  If you wedge too much you will lose the 'speckle' to a more uniform 'tint'.

 

LT

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.