bluecreekpottery Posted June 23, 2017 Report Share Posted June 23, 2017 Glaze cracks Link to comment Share on other sites More sharing options...
Mark C. Posted June 23, 2017 Report Share Posted June 23, 2017 This photo does not show them well-or at least I cannot see them well Is this photo of a Pitcher plant inside? Link to comment Share on other sites More sharing options...
Marcia Selsor Posted June 23, 2017 Report Share Posted June 23, 2017 looks like a bloating issue from a chunk of something in the clay. As suggested in your other post, break one open and find out . What clay or type of clay are you using. Marcia Link to comment Share on other sites More sharing options...