Spot On Bisque

Recommended Posts

I had about 50 mugs in the kiln.  Bisque load, speckled buff, Laguna, fired to 04.  There were 3 mugs that had spots like this on them.  It's almost pitted.  It looks like iron or something.  Any thoughts?

 

Robertapost-14790-0-27844700-1497564744_thumb.jpg

Share this post


Link to post
Share on other sites

Laguna clay from their California plant can have lots of crap in it. I've pulled out matchstick size pieces of wood, metal bits, and small bits of plastic. Maybe from this?

Share this post


Link to post
Share on other sites

Laguna clay from their California plant can have lots of crap in it. I've pulled out matchstick size pieces of wood, metal bits, and small bits of plastic. Maybe from this?

could be.  It looks like iron to me.....this spot is the largest.  This is the last of this particular batch.  Let's hope the next 300 pounds is better. 

Share this post


Link to post
Share on other sites

My helper just found a piece of wood that was about 2 inches x1/2 inch in our porcelain from Laguna.

When you go thru many tons per year its always going to turn up some crap. Iron burn outs are common in my past 40 years.

You can grind it out with a dremial then patch 

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.