Is there an easy way to convert this cone 10 glaze to cone 6?

 

Phils 103 White

F4.................51

Dolomite........15.6

Magnesium carb..5.7

EPK...............17.1

Silica..............10.6

Zircopax......... 10

Share this post


Link to post
Share on other sites

If you are looking for a dolomite matte instead of trying to alter that ^10 one you could try this one that is formulated for ^6. For me it's too matte as is but if you do a line blend with a clear that fits your clay you should be able to get there. 

 

"Is there an easy way...."

haven't found an easy way with anything to do with clay  ;) 

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now

×

Important Information

By using this site, you agree to our Terms of Use.