here is one I used in Oxidation or reduction. Can't say whether it will work with Standard 266. It worked with ^6 porcelain and stoneware. semi gloss



Clear ^6

Neph  Syen      26.1

Gerstley Bor.      4.7

EPKaolin          19

Whiting             18.7

Silica                 31.5