Ryan_pelo Posted May 15, 2017 Report Share Posted May 15, 2017 I was trying out the Alberta slip rutile blue glaze. 40% Alberta slip 40% Alberta slip calcined 20% Frit 3134 + 4% Rutile I tried a glaze with just the base, no rutile, and it turned out great, no running. Then on another column I have the glaze with the rutile and it runs like crazy, all the way down the column and it pools at the base. My ceramics teacher has another similar glaze with a different recipe that looks almost the same and uses the same rutile mechanism to produce the variegated blue, but it works just fine without running. I thought I messed up the batch so I remade it and I still got the running, It's bizarre. I don't think rutile has caused problems like this in my other glazes. Why is this happening? What would decrease running, increasing the frit or decreasing the frit? Link to comment Share on other sites More sharing options...
High Bridge Pottery Posted May 15, 2017 Report Share Posted May 15, 2017 Very bizarre that adding 4% rutile would change a glaze that much. Are you sure nothing went wrong mixing the recipe or in a much hotter place in the kiln? Reducing the frit should reduce running. Link to comment Share on other sites More sharing options...
Callie Beller Diesel Posted May 15, 2017 Report Share Posted May 15, 2017 No, you're correct: rutile does that in some cases. Normally it's fluxing action is pretty minor, but when you throw it in with iron, which there is a lot of in Alberta slip, they both flux out more than they normally would. This glaze is a bit problematic because it requires a thick application to work, which can exacerbate things. Also, the fluxing action is part of what helps create that floating part of floating blue, so adjusting the frit could reduce some of that really pretty effect. Something that might help your issues would be to change Frits from 3134 to 3124. 3124 has more Alumina, which will make for a stiffer glaze. Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.