This is a porcelain made with 50% T-6 kaolin & 55% milled anoka sand and the Celadon glaze uses 56% anoka sand  and together it makes a really good matching combo  the glaze just glows with a soft  blue green. I hope to start making some work with this combo now  . Reduction fired to cone 8 