O,K i got a bag of 325 custer from continental clay in minneapolis Minnesota in march  2017 i sent in some to get analyzed by ALS global.  i put pictures of the sheet in case you think i am fooling you  it is not what is listed on the web site it is sample NO .5 the others are anoka sand  i am working  with . Hear is the current analysis of Custer feldspar  72.47 silica 15.24 alumina, .27 Iron. .25 calcium , .08 MG,  3.45 sodium, 7.42 K20  0.01 titanium .26 phosphate it is a potassium granite so make your changes as needed  , fellow potters

post-80534-0-93599900-1490925731_thumb.jpg

post-80534-0-55538700-1490925808_thumb.jpg

post-80534-0-93599900-1490925731_thumb.jpg

post-80534-0-55538700-1490925808_thumb.jpg

Share this post


Link to post
Share on other sites

Kaolinwasher, thanks for checking into this. I am not the slightest bit surprised at this, actually I am perversely comforted that the rant I have been on for at least 5 years is still borne out by yet more evidence. Your numbers are very close to Ron Roy's published findings several years ago and my data from 2012. As I have said before, I don't mind that the numbers change over time. It's a natural material and Mother Nature moves. What I mind is that Pacer continues to insist that there is no change in the analysis from 10 years ago.

anchorman likes this

Share this post


Link to post
Share on other sites

ALS global's method "ME-XRF06" is an X-Ray Fluorescence analysis of a fused bead -- a typical method for a "whole-rock" "major element" geochemical analysis of pulverized rocks. The powdered sample is mixed with a lithium borate flux, melted, and then cast into a glass disc, which is then analyzed with a wavelength dispersive XRF spectrometer....

terrim8 likes this

Share this post


Link to post
Share on other sites

I just talked with Mike ,at continental clay where i got the 325 mesh custer  and he said that that load was from june of 2016 and they just got a new load in . he said they had problems with the jasper stone lining in the ball mill that was contaminating the feldspar  a wile back . But mike said they always figured custer for having 8% potash and not to pay attention to the posted amounts on Custers Web site . But it has changed  as Ron roy posted and now my analysis  it seems to be staying the same since 2000 and 2012 and 2016  its a good material and i would not stop buying it  my problem was i just want to know whats in it so i can make my calculations. Also mike said you can get the analysis from them on every new load which may change a little but is close to what i got and ron roys.

terrim8 likes this

Share this post


Link to post
Share on other sites

This is my latest body test using the new Custer feldspar.   25% T-6 kaolin  25 champion ball clay,25 Custer feldspar and 20% Purple sioux quartzite,  It vitrified, did not craze,  did not boat . it does have some tiny Iron specks,  But if I used 25 i think it would have broke on cooling  now with the new 72.47 silica in custer . The tests on the bottom left and right are stone  tests , The one on the right is a magic rock , and it flattened out nice. Its from a huge bolder , have to get more of that . One thing i did is make sure i bisqed to cone 04 in oxidation  that seems to have eliminated the blistering of the clay body. 

post-80534-0-97923000-1491061234_thumb.jpg

post-80534-0-97923000-1491061234_thumb.jpg

Share this post


Link to post
Share on other sites

I have been liking the custer feldspar . I got a porcelain to work very well with it   25 T-6 25 champion ball clay . and 25 custer and 19 flint with 1% Iron  very good body for chin blue and that typ of glaze . plus its granite composition makes it useful for many glazes. I know it cost more to froth float out the feldspar  which would give something like Mahivar in composition  so they have probably went for the cheeper option of just leaving the quartz in one reason its less expensive. but still a Dang good spar  I like it  hope they keep it the same  Gunnar R 

Share this post


Link to post
Share on other sites

I'm wondering if the test method used by pacer and whatever is used by plainsman clays is different than the one mentioned above and whether that is responsible for the discrepancies with the test done for kaolinwasher?

https://digitalfire.com/4sight/material/custer_feldspar_253.html

I had reps from resco tell me to my face that goldart didn't have a sulfur problem, but testing revealed that it was at least 10x higher in sulfur content than the fireclay we used at the time.  And mine eyes and nose didn't lie to me when I smelled it coming from the kiln and saw the damage it was doing to the kiln with every firing.  Goldart gone, sulfur problems gone.

I'm going to bring some of the custer feldspar we have to a lab and see what they say the potash content is, I guess.  There are people who do soil testing and such at the university where I work who have helped me in the past.

Thanks for having the tests run that you did, and sharing them with us!

 

Share this post


Link to post
Share on other sites

The information on digitalfire is not based on their own independent lab testing for all those materials, but is whatever the producer published. The problem with Custer is Pacer refuses to acknowledge that current laboratory testing consistently reveals that the content of the material they are selling now is far different than the material they were selling 10 years ago, and thus they continue to publish the obsolete materials analysis.The exact ceramic oxide content doesn't matter to their main customers (e.g., paint, rubber, and abrasives industries) so they just obfuscate.

Share this post


Link to post
Share on other sites

"The chemical analysis of a load received in Nov 2013 reports 10.1 K2O, 3.1 Na2O and 0.1 Fe2O3 (which very closely matches their reported numbers)."

 

This made me think they had sent out sample(s) for testing at some point. I could be reading that wrong, though.

Share this post


Link to post
Share on other sites

they must grab one pure chunk of feldspar frome the mine and it would give that number . if they are that far off that is some horrible variation,  i would tend to beleive somthing funny is going on  i like the new custer granite  anyway  hope they keep it the same

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now

×