This is my small jaw crusher i use for crushing ,Granite, sioux quartzite, that i use in my glazes and clay bodies mine came with a badd toggle bolt  that i need to fix  otherwise its a fine machine  i was crushing the St Cloud granite, and my friend was filming the company that sells them is called 911 metelergical  this one will run you 500 but i think they have a kit  you assemble for less i do not work for  or sell them myself 