I just bought an easy fire e18s kiln. I was going to do a test fire. I have one question. The instruction manual talks about spring hinges and things. We didnt disassemble the kiln. Do we need to follow any of these steps? We simply assembled the stand and placed the kiln on top. Am I ready for test fire?

Share this post


Link to post
Share on other sites

That kiln does not have the spring hinges. It doesn't need them since it's so small. You do need to make sure that the kiln is not rocking on the stand. Put sheet metal shims under the feet of the stand as needed to get it sitting evenly on all feet. Open the control panel and make sure all the connections are still tight. Make sure all the elements are seated into the holders, especially at the corners. Then you're ready to fire.

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.