Dani Posted February 20, 2017 Report Share Posted February 20, 2017 There is one shelf where the kiln wash flakes off every time it is newly applied. The other shelves, where the kiln wash is applied the same way, do not have this problem. Any suggestions? Link to comment Share on other sites More sharing options...
neilestrick Posted February 20, 2017 Report Share Posted February 20, 2017 Try going over it with a grinding disc (lightly). Could be there's a thin layers of something on the shelf preventing the wash from binding. The grinder may also make the surface a tiny bit rougher, allowing the wash to grab better. Link to comment Share on other sites More sharing options...
Marcia Selsor Posted February 20, 2017 Report Share Posted February 20, 2017 if you have a wire brush disc for a drill, that won't dig into the shelf and may remove whatever the problem is. Either method will create a lot of silica dust. Wear safety googles and good dust mask. You may also want to wear a hat. Marcia Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.