Good morning, I am new to electric kiln firing and as such kiln wash. Bought some that was mixed from a local studio and applied 3 coats. First one may have been a little thick so I thinned up the latter coats. After drying each layer I have noticed some cracking on the surface. What should I do ? Should I sand it till no longer visual. It is sparatic on some but not all of the shelves.

Planning on doing a bisque fire soon.

Thanks so much for help !!

Share this post


Link to post
Share on other sites

I would sand or scrap it all off before firing it. It comes off easy now. Thin the wash and apply two thin coats. It's cracking now as it's to thick.let it dry between coats. Most apply wash two thick and it cracks.

Share this post


Link to post
Share on other sites

A lot of kiln wash is made to be as cheap as possible. If you find your wash is flakey after firing you might want to mix up your own. 

 

This works well:

 

50 alumina hydrate

25 epk

25 calcined epk

Share this post


Link to post
Share on other sites

Something I stumbled upon when starting out, but have not seen it discussed by the experts - I originally used a recipe similar to the one Marcia posted, and sometimes had serious peeling and other times not. Then I noticed that the peeling shelves were all ones laid flat on the table and left to dry while the non-peeling ones were leaned against the wall at an angle, exposing the back side as well as the front side. I assumed it had something to do with allowing moisture to penetrate through the shelf and evaporate from the back rather than all of it needing to come back out only the front after the coating of wash on the surface was already dry. I now always prop the freshly washed shelves against something while they dry. I have also changed my wash recipe to one Min suggests to eliminate the silica and replace half the kaolin with calcined kaolin to eliminate shrinkage. Have not had any problems with this.

Share this post


Link to post
Share on other sites

Does the surface of the shelves affect the flaking of kiln wash? The shelf where this keeps happening appears to be more smooth and vitrified than the other shelves where flaking does not happen.

Share this post


Link to post
Share on other sites

Thinking of buying another shelf for more options when packing. Does a newly Kiln Washed shelf need to fired first before use, or is it ok to put ware onto the fresh wash?  I'm using commercial kaolin/al hydrate premix. Assuming also I can trust my glazes enough not to run before the shelf is protected.

 

Joe

Share this post


Link to post
Share on other sites

Thinking of buying another shelf for more options when packing. Does a newly Kiln Washed shelf need to fired first before use, or is it ok to put ware onto the fresh wash?  I'm using commercial kaolin/al hydrate premix. Assuming also I can trust my glazes enough not to run before the shelf is protected.

 

Joe

 

If your glazes don't run and you have used them a lot(trust) then you don't have to have kiln wash. I am buying three new shelves for plates and I have no plans on putting kiln wash on them as the glazes I will use for plates will not run. I think several potters here don't use kiln wash on their shelves because they work with the same glazes for their production and they know it won't run.

 

This might not be true if your using porcelain compared to stoneware as some porcelain can get sticky and parts of the feet can stick to the shelves.

Share this post


Link to post
Share on other sites

I use Highwater Clays cone 6 Little Loafers white clay and it will definitely pluck if I don't wax, kiln wash and sometimes even use kiln washed cookies so the amount of foot ring in say something like a large platter is limited in its contact with the shelf. I don't have any real issues with my glazes since I know them and am real careful but I am getting ready to redo the kiln wash on all my shelves because I have noticed it is starting to flake off more and more.

 

T

Share this post


Link to post
Share on other sites

Thanks Joseph for reminding me that wash is optional. 

 

I DO want to wash the shelf so that it is prepared for any glaze drips in subsequent firings. My question was whether I can put some (trusted drip-safe) ware on the unfired kiln wash the first time its fired or whether the wash MUST be fired without ware initially.

 

The kiln wash mixture has kaolin which I guess acts as a binder to keep the alumina hydrate attached to the shelf so if I put ware on before it has fused during the shelf's first firing I don't want it to bind to the ware as well. I imagine a problem is unlikely as conditions in the foot ring/kiln wash/shelf contact area will be the same in all the subsequent firings.

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.