Marcia Selsor    1,301

you could try Sairset refractory cement. I am getting a pint to repair one of my kiln lips and the top layer of bricks. they had a tough trip from texas. it is $10 at Archie Bray for the smallest quantity , a pint.Call and ask them what they think or google the product.

.

 

Marcia

Share this post


Link to post
Share on other sites
oldlady    1,323

saw a wonderful idea on pinterest.  fold a slab into 3 like folding a letter to fit into an envelope.  but hold the sides at 90 degrees from the bottom.  poke holes in the sides so you can run your bead wire through the holes on both sides to hold the beads.

 

that was a busy day and the brain was tired.  the shape of the slab is a big U.  the holes were placed in the upright part and were all over so different sized beads could be fit anywhere.  the U looked about 4 inches wide with about a 6 inch bottom of the U.

Share this post


Link to post
Share on other sites
neilestrick    1,378

You can't mortar together refractories like bead trees or kiln posts. Get new ones or make your own.

 

Used kiln bricks are also difficult to mortar back together. New bricks are easier to get a good bond. Marcia, the best I've found for repairing old bricks is the phosphate cement that L&L sells. This isn't just a plug for L&L, I've actually had way better luck with it than typical refractory mortars, of which I've tried several. There's a reason they put it in their repair kits. It isn't cheap, but it works.

Share this post


Link to post
Share on other sites
Pugaboo    438

I make my own out of my regular LL clay and they have so far lasted through many many firings. It's way cheaper and I can custom make them in a size and shape to meet my needs. This is what I would do rather than risk a repair failing.

 

Think I posted pictures of mine on here at one point in the past.

 

T

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×