tanyamatix Posted January 25, 2017 Report Share Posted January 25, 2017 Hi, I was wondering if anyone has used MN Clay's Potters Pads (it's an underglaze stamp pad) without glaze. I want to use it on the exterior of a bowl that will be washed often. I don't want to glaze the exterior but need to stamp a logo on. Will the unglazed underglaze chip/get washed off. I am firing to cone 7 which is within the firing range of the underglaze. Thanks! Tanya Link to comment Share on other sites More sharing options...
Joy pots Posted January 25, 2017 Report Share Posted January 25, 2017 It's permanent, I use the underglaze pens & have the refill that would be used in the pad. I've used it to sign the bottom of pots where no glaze is applied. Joy Link to comment Share on other sites More sharing options...