Kaolinwasher Posted December 4, 2016 Report Share Posted December 4, 2016 This is my small propane kiln , its inside is 6.5" wide x 9" tall but the fire comes under the shelf so i lose 2.5" with that and the shelf . the walls are 2.5" 2600 insulating brick and 1.5" of fiber board. very nice . the reduction is tricky i have found i must keep a blue flame coming out and be patient. until the cone starts bending then i can back off the restriction to raise temp https://www.youtube.com/watch?v=W1-ZgA9BdtE Link to comment Share on other sites More sharing options...
Marcia Selsor Posted December 4, 2016 Report Share Posted December 4, 2016 nice! is that what you fired in the other post? Marcia Link to comment Share on other sites More sharing options...
Guest JBaymore Posted December 4, 2016 Report Share Posted December 4, 2016 Nice little setup there. best, ............john Link to comment Share on other sites More sharing options...
NancyAmores Posted December 5, 2016 Report Share Posted December 5, 2016 Liked and Subscribed! Will be following your results as I'm hoping to do something similar in a few years. Thanks for the uploads, they'll be very useful. Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.