Well I'm ordering My next years materials

I have a few items for other potters materials on this list like the stoneware white bodies

and some small quantity materials in 10# increments 

It looks like about 23,000 lb order for next year-good thing I'm slowing down-as my back is hurting looking at moving this into my clay shed which has less than a ton left right now.

I think I'm covered  well but you may see something I'm missing??

I'm also doing a (B) order for another potter-small order of a ton of Porcelain

This stuff will come in January

 

Liscom Hill Pottery Order (A)

 

Material- Cone 10 wet bagged clay

 

4 Tons WC 384 Dave’s Porcelain newest stock on floor Pent-#6 ¼

6 Tons WC 383 Dave’s Porcelain-pent #6 Special order

1000#s WC 631 550 Porcelain-newest stock on floor

500#s  WC 428 Babu Porcelain-newest stock on floor

200# WC 841 Danish White plain

500#  WC 842 Danish White W/sand

 

250# WC 419 wood and sagger clay IF Available ? Small chance

 

 

Dry materials (A)

 

10# Zircopax plus

10# Spanish red Iron oxide

10# Red NR-R-02

10# Alumina Hydrate

20# cobalt Oxide

50# custar feldspar

50# 325 mesh silica

100#s Nepline syenite A-270 (50# bags)

100#s whiting

2 bags Alberta slip (44# bags)

 

1 FS243 protection tube

1 FS 24012 thermocouple with block

15 -4 inch triangle posts (4 inch long X 1 ½ ) Please do not send square posts

15 -3 inch triangle posts  (3 inch long x 1 ½ ) Please do not send square posts

15 -1 inch triangle posts (1 inch long X 1 ½ ) Please do not send square posts

Share this post


Link to post
Share on other sites

You can fit more work around the triangle posts as the have an angle edge.Square post take up more room. Since I load on average 35-40 shelves per fire this little bit adds up. as it 3 posts per shelve. Bowl rims can get closer to stilts  as well as all other forms. The tri posts (this are the larger 1 1/2 inch ones) not the small hobby kiln ones .Loading is an art in itself and is not spoken about much.

I own lots of posts(square round tri whatever) and over time they compress meaning they are no longer what they started out.

Thats why I am ordering more.

At cone 11 with a 5 foot vertical load on them and 25-30 glaze fires a year after 20-30 years the post are shorter and I get feed up mixing and matching posts to keep it all flat.

I coat the ends with wash as well.

I have 4 racks racks of post one at each kiln

This one next to car kiln has various size cubicles that are made for each size from small to longs.

post-8914-0-81455900-1479591769_thumb.jpg

Share this post


Link to post
Share on other sites

aaah Mark. thanks for the lengthy explanation. it all makes sense now. i have been allowed to help load the kiln. and before i put the posts in i have to size them and make sure they are the right height. i wondered why they shouldnt be. but the lab tech was focused on organizing loading the kiln so i didnt want to break her concentration. 

 

triangle is space consideration. wow. woudlnt even have thought of that. our school has all kinds too but mostly triangular ones. 

Share this post


Link to post
Share on other sites

Mark:

I have gotten so good at mixing things: perhaps I should try some lithium carbonate based analgesic. Remember, you have to test.test.test....Thought 2: place an ad at your local community college for a "day with a production potter."   Leave the details out until the class arrives.

Nerd

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.