What brand of underglazes are you using?

I find with the Mayco ones, the binder in them resists glaze, and you'd be wise to re-bisque. That said, I just saw a Mariko Paterson demo, and she mentioned if you give your pots a quick rinse before decorating, the slightly dampened pot will help draw the underglaze into the pores. I haven't personally tested this yet though.