Does any one know where I can purchase an affordable motorised pestal and mortar.

I saw them being used in Shigaraki, haven't seen them any where since.

I'm adding oxides to terra sigilatta and need a finer particle size.

Any help would be appreciated

Link to comment
Share on other sites

Guest JBaymore

Unfortunately, there is a lot of equipment I've seen when I've been working in japan that is not easily available in the US.  Some nice "toys".  I've seen those same units at Tokyo University of the Arts when I've been there.

 

I'll check my Japanese equipment catalogs and see what I can find.  But they will almost for sure be expensive to start with, and also expensive to import.

 

best,

 

.............john

Link to comment
Share on other sites

there was an article once in ceramics monthly showing someone using a small motor mounted on a piece of wood with a belt  running around a jar that rested on 4 wheels.  the jar was a ball mill when it was filled with marbles.  bruce, our intrepid internet searcher, could probably find it.

Link to comment
Share on other sites

Archived

This topic is now archived and is closed to further replies.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.