Earthenware Vs Stoneware

Recommended Posts

What do ya'll think? If I fire earthenware and stoneware both to ^06 which will be most durable?

I want to burnish the piece, bisque fire it then smoke it in a metal can, which of these, earthenware or stoneware,

will take the smoke better?

Share this post


Link to post
Share on other sites

What do ya'll think? If I fire earthenware and stoneware both to ^06 which will be most durable?

I want to burnish the piece, bisque fire it then smoke it in a metal can, which of these, earthenware or stoneware,

will take the smoke better?

 

 

Beware! Some earthenwares will melt into a puddle at ^6, while some stonewares will not mature at that temp. If you burnish an earthenware piece, then fire it to ^6, it will lose most of the shine, though it will still be relatively smooth. If you fire to ^6, the clay closes up too much to accept the smoke from a pitfire. If you bisque low, its my experience that either clay will smoke nicely, both red clays and white, though of course the whites are more dramatic.

Share this post


Link to post
Share on other sites

What do ya'll think? If I fire earthenware and stoneware both to ^06 which will be most durable?

I want to burnish the piece, bisque fire it then smoke it in a metal can, which of these, earthenware or stoneware,

will take the smoke better?

 

 

Earthenware should be more durable. Check with your supplier, you might want to fire just a little higher. You can read an article on the durability of different clays here:http://www.potters.org/subject87702.htm

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×