Has anyone used any of the greys for mason stains? I am looking for a nice pale grey, everything I do with 6600 and  white is just too dark for what im looking for or it just isn't grey at all, more of a brown. if anything I would like it to be more greenish grey then blackish grey is that makes sense?

 

 

Has anyone tried the Taupe? 6503? Probably what im looking for the most. Trying to make some sort of crackle grey glaze for some jars I am making.

 

S0BlldG.png

Link to comment
Share on other sites

Are you starting with a base glaze that is already white? What makes the glaze white? That element might be affecting the stains result.

 

If your result it too dark, try using less. My gray glaze uses a teeny amount, 0.7% stain.

Link to comment
Share on other sites

For me, 6600 tends towards green when used in tiny amounts. I don't get a brown at all. This is in a glaze that is opacified with Talc and Neph Sy, and maybe the calcium in the Wollastonite.

 

When used with Titanium it's even more green and towards olive green. When used with Tin it makes a very neutral gray, maybe a tiny hint of blue, and once in a while a tiny hint of pink (Chrome and Tin sometimes makes pink.)

Link to comment
Share on other sites

I think that is my problem. I was using it with a Tin glaze, which was making just a grey, which wasn't interesting or anything, and I think the tin made it hint brown when thin(maybe?). I am going to try the talc neph sy thing. 

 

I am trying to nail down my 5 glazes. I have 2 I really love, just gotta get 3-4 more that go well. I am trying to find some sort of faint greyish green crazed glaze and a whiteish grey glossy. Once I get those two down. I will be a lot happier. I am close, going to run a bunch of currie grid test the rest of this month to find the area I am looking for. 

 

Thanks for color's based on ingredients hues.

Link to comment
Share on other sites

If you can find  Mason Stain #6523 "Soft Green Grey", it may be a good answer for you.  It's listed on the Mason Color website as a mix of 6% 6609 and 94% 6700. I assume they do not mix the #6523 any longer. But I still can get it at Sheffield Pottery in Sheffield, MA .  http://www.sheffield-pottery.com

It's is a beautiful light grey with a green cast. The color displayed on the Sheff. Pot. website is much darker than my results mixing 5% stain into porcelain slip with 10% zircopax added. I use it as a slip over porcelain and carve through designs through the slip. There is no problem with a clear glaze that has zinc.

 

You'll find interesting info on the Mason Color website FAQ page about how to mix and troubleshoot. 

Link to comment
Share on other sites

If you can find  Mason Stain #6523 "Soft Green Grey", it may be a good answer for you.  It's listed on the Mason Color website as a mix of 6% 6609 and 94% 6700. I assume they do not mix the #6523 any longer. But I still can get it at Sheffield Pottery in Sheffield, MA .  http://www.sheffield-pottery.com

It's is a beautiful light grey with a green cast. The color displayed on the Sheff. Pot. website is much darker than my results mixing 5% stain into porcelain slip with 10% zircopax added. I use it as a slip over porcelain and carve through designs through the slip. There is no problem with a clear glaze that has zinc.

 

You'll find interesting info on the Mason Color website FAQ page about how to mix and troubleshoot. 

Link to comment
Share on other sites

Archived

This topic is now archived and is closed to further replies.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.