Are Cone 5/6 Ceramics Correctly Referred To As "stoneware"?

Recommended Posts

Now that I have my own studio and electric kiln, I'm moving from cone 10 clays to cone 5. This new world of mid-range clays, glazes, and firing is like starting all over again.

 

I'm uncertain about whether cone 5/6 ceramics are correctly referred to as stoneware. Pretty sure that the term "earthenware" refers to low-fire ceramics, but I await the wisdom of those who know better about these things. :-)

Share this post


Link to post
Share on other sites

Thank you, Neil. My main concern with the terminology is how I refer to my pottery, say, when I'm posting items on Etsy or describing pieces to buyers at shows. But I am still in that gray area working both with cone 5 and 10, where I have to be careful of which pieces I will glaze fire and which will be taken to my old membership studio for cone 10 firing!

 

:)

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.