Firing Bisque & Glazed Pieces Together


Recommended Posts

I have two earthenware pieces were glazed and fired but they didn't come out to my liking. I'm not working with any more low fire clay but have a load of cone 5/6 pieces ready for bisque firing. Can I reglaze my two low fire, earthenware pieces and put them in the same load with my bisque ware and fire to cone 05? I'm not sure if the speed (slow) and the burnout of organic matter in the bisque firing process will affect the glaze on my two pieces.

Link to comment
Share on other sites

put the glazed pieces in the cooler part of your kiln.  if you do not know where that is, put them on the bottom shelf.  that way, if anything in the raw ware does have something bad to burn out, it will be above the pieces you are worried about.