When I glaze tiles I pour the glaze on them.  I have a plastic box I put a rack in, cover each tile with glaze I usually use and plastic measuring cup with a spout.  I let the tiles dry where they are.  You can reuse the glaze in the bottom of the box, you might have add some water to it.  Denice