Declan Posted June 3, 2016 Report Share Posted June 3, 2016 Hello, I have a series of large 1 1/2lb tiles which I want to permanently fix into a deep picture frame. What is the best glue to use given the weight of the tiles and that it will be fixed to picture frame backing. Thank you, Declan Link to comment Share on other sites More sharing options...
Marcia Selsor Posted June 3, 2016 Report Share Posted June 3, 2016 I use mortar but liquid nails would work on that scale. Marcia Link to comment Share on other sites More sharing options...
Declan Posted June 3, 2016 Author Report Share Posted June 3, 2016 I use mortar but liquid nails would work on that scale. Marcia Thanks Marcia Link to comment Share on other sites More sharing options...
Biglou13 Posted June 3, 2016 Report Share Posted June 3, 2016 what about larger tiles 9# ish ? Link to comment Share on other sites More sharing options...
rakukuku Posted June 3, 2016 Report Share Posted June 3, 2016 JB weld epoxy is pretty good. takes awhile to set up. also gorilla glue epoxy sets up fast. rakiki Link to comment Share on other sites More sharing options...
glazenerd Posted June 3, 2016 Report Share Posted June 3, 2016 Good ole clear silicone works just dandy. Nerd Link to comment Share on other sites More sharing options...
paradisegold Posted July 7, 2016 Report Share Posted July 7, 2016 Hi... Now many hardware liquid to help easy and quick set up for ceramic tiles. Link to comment Share on other sites More sharing options...
perkolator Posted July 15, 2016 Report Share Posted July 15, 2016 For something like this you could use almost anything. Hot glue, E-6000, silicone caulking, liquid nails, etc. Heck, you can even just use those staples/brads to hold it in the frame. Just make sure the FRAME is up to the task. Link to comment Share on other sites More sharing options...