Can anyone recommend a good cone 6 crater glaze?

The clay in this picture is a cone 6 porcelain and the glaze is a commercial clear cone 6 glaze with some fine 200 mesh silicon carbide added. Maybe i started with too much silicon carbide- I'm trying for a clear crater glaze. I have a recipe for cone 9 crater glaze that does not use silicon carbide but not cone 6.

 