nancylee Posted May 21, 2016 Report Share Posted May 21, 2016 Hi all, I glazed B Mix, cone 5 with cerulean underneath and celadon froth above. There is an area where the glaze didn't flow, right near the bottom. It's like a glaze skip. Can I reglaze this? If so, how? Also, I have a green mug that I glazed with a brush and there are ugly brush marks. It's a cone 5,6 glaze. I should know this, but can't remember. Thanks much, Nancy Link to comment Share on other sites More sharing options...
Mark C. Posted May 21, 2016 Report Share Posted May 21, 2016 Warm the piece and reglaze the bare spot and add more glaze via dipping or brushing and refire. Link to comment Share on other sites More sharing options...
Joseph Fireborn Posted May 22, 2016 Report Share Posted May 22, 2016 Marko just made a post about this: http://community.ceramicartsdaily.org/topic/14342-re-glaze-tip-of-the-day/ Link to comment Share on other sites More sharing options...
nancylee Posted May 22, 2016 Author Report Share Posted May 22, 2016 Thank you! Much appreciated! Nancy Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.